Taber test
Proven by scientific tests!
Finitec finishes give the best results at the Taber test, far ahead competition. After 1000 rotations, the aluminium oxide finish Finitec 9000 only lost a mass of 2 mg; it is the most resistant finish of the industry!

Taber test (test ASTM D-4060)
The Taber test measures wear resistance of finishes and varnishes. An instrument called abrasiometer inflicts a continual friction to the finish with an abrasive disk. The tested sample is weighted before and after the test in order to measure its loss of mass.